The paper presents experimental results directed on the development of new empirical criterion for multiaxial fatigue. The proposed criterion may be applied for materials responding the cyclical loading by the formation of deformation relief, i.e. system of extrusions, intrusions, persistent slip bands. The tests were carried out on aluminum alloy D16AT, the aluminum cladding layer of which is able to react cyclical loading by formation and evolving of relief pattern.

Article Details

Section

Articles

References

1. Kenmeugne B., Soh Fotsing B. D., Anago G. F., Fogue M., Robert J.-L., Kenne J.-P. On the evolution and comparison of multiaxial fatigue criteria. International Journal of Engineering and Technology. 2012.Vol. 4. № 1. P. 37–46.

2. Karuskevich M. V., Radchenko A. I., Zasimchuk E. E. Single-crystal as an indicator of fatigue damage. Fatigue Fract. Engng. Mater. Struct. 1992. Vol. 15. № 12. Р. 1281–1283. https://doi.org/10.1111/j.1460-2695.1992.tb01263.x

3. Karuskevich M., Karuskevich O., Maslak T., Schepak S. Extrusion/intrusion structures as quantitative indicators of accumulated fatigue damage. International Journal of Fatigue. ISSN: 0142-1123. 2012.Vol. 39. P. 116–121. https://doi.org/10.1016/j.ijfatigue.2011.02.007

4. Karuskevych M. V., Zhuravel’ I. M., Maslak T. P. Application of Fractal Geometry to the Problems of Prediction of the Residual Service Life of Aircraft Structures. Materials Science. ISSN: 1068-820X2012. Vol. 47. Issue. 5. P. 621–626. https://doi.org/10.1007/s11003-012-9436-7

5. Karuskevich M. V., Vogt J. B., Serre I. P., Maslak T. P. Surface relief sensor for Structural Health Monitoring. Fatigue behaviour: from specimen to structure (JIP 2013): 13-the intern. spring meeting, 22-23 May 2013. Paris: 2013, P. 18.

Most read articles by the same author(s)